C. Cabrera Sanchez. "Sustitución del agregado fino por Policloruro de Vinilo en el concreto estructural," tesis de licenciatura, Fac. de Ingienería, Univ. USAT, Chiclayo, Perú, 2023. [En línea]. Disponible en: (es_PE)
RTU006901
http://hdl.handle.net/20.500.12423/7218
Este artículo es de tipo experimental, ya que se evaluó el comportamiento que tiene el concreto estructural al agregarle PVC en sustitución del agregado fino en un 20%, 30% y 40%. Se determinaron las propiedades físicas del policloruro de vinilo (PVC) y los agregados (fino y grueso), obteniendo que el peso específico del PVC es de 1.14 gr/cm3 y del agregado fino es de 2.59 gr/cm3. Se hicieron pruebas de granulometría, peso específico, contenido de humedad, resistencia a la compresión, flexión y tracción. Del mismo modo se desarrolló un concreto patrón y concretos reemplazando el agregado fino en ciertas cantidades de PVC triturado. Como resultado de los ensayos de resistencia a la compresión se tiene que para el concreto patrón la resistencia es de 242 kg/cm2, para un concreto teniendo un 20% de PVC es de 214 kg/cm2, para un 30% de PVC es de 209 kg/cm2 y para un 40% de PVC es de 153 kg/cm2. Para la prueba de resistencia a flexión a mayor porcentaje de PVC la resistencia tiende a disminuir, pero estando dentro de los límites permitidos de la norma técnica. (es_PE)
This article is of an experimental nature, since the behavior of structural concrete was evaluated by adding PVC to replace the fine aggregate by 20%, 30% and 40%. The physical properties of polyvinyl chloride (PVC) and the aggregates (fine and coarse) were determined, obtaining that the specific weight of PVC is 1.14 g/cm3 and that of the fine aggregate is 2.59 g/cm3. Tests were carried out on granulometry, specific weight, moisture content, compressive strength, flexural strength and tensile strength. In the same way, a standard concrete and concretes were developed by replacing the fine aggregate with certain quantities of crushed PVC. As a result of the compressive strength tests, for the standard concrete the resistance is 242 kg/cm2, for a concrete with 20% PVC it is 214 kg/cm2, for 30% PVC it is 209 kg/cm2 and for 40% PVC it is 153 kg/cm2. For the flexural strength test, the higher the percentage of PVC, the resistance tends to decrease, but is within the limits allowed by the technical standard. (es_PE)
application/pdf (es_PE)
spa (es_PE)
Universidad Católica Santo Toribio de Mogrovejo (es_PE)
info:eu-repo/semantics/openAccess (es_PE)
http://creativecommons.org/licenses/by/4.0/ (es_PE)
Concreto estructural (es_PE)
Agregado fino (es_PE)
Resistencia a la compresión (es_PE)
Structural concrete (es_PE)
Fine aggregate (es_PE)
Compressive strength (es_PE)
Sustitución del agregado fino por Policloruro de Vinilo en el concreto estructural (es_PE)
info:eu-repo/semantics/bachelorThesis (es_PE)
Universidad Católica Santo Toribio de Mogrovejo. Facultad de Ingeniería (es_PE)
Ingeniería Civil Ambiental (es_PE)
Bachiller en Ingeniería Civil Ambiental (es_PE)
PE (es_PE)
http://purl.org/pe-repo/ocde/ford#2.01.00 (es_PE)
http://purl.org/pe-repo/renati/nivel#bachiller (es_PE)
32965940
https://orcid.org/0000-0002-3631-2001 (es_PE)
74620339
732026 (es_PE)
Lopez Carranza, Atilio Ruben (es_PE)
http://purl.org/pe-repo/renati/type#trabajoDeInvestigacion (es_PE)
Privada asociativa



This item is licensed under a Creative Commons License Creative Commons