Bibliographic citations
This is an automatically generated citacion. Modify it if you see fit
Saldaña, P., (2018). Resistencia a la compresión de un concreto compactado con rodillo en diferentes tiempos de vibrado [Tesis, Universidad Privada del Norte]. https://hdl.handle.net/11537/12739
Saldaña, P., Resistencia a la compresión de un concreto compactado con rodillo en diferentes tiempos de vibrado [Tesis]. PE: Universidad Privada del Norte; 2018. https://hdl.handle.net/11537/12739
@misc{renati/521486,
title = "Resistencia a la compresión de un concreto compactado con rodillo en diferentes tiempos de vibrado",
author = "Saldaña Saldaña, Piere Andreé",
publisher = "Universidad Privada del Norte",
year = "2018"
}
Full metadata record
Ravines Azañero, Irene Del Rosario
Saldaña Saldaña, Piere Andreé
2018-02-08T22:53:19Z
2018-02-08T22:53:19Z
2018-01-05
Saldaña, P. A. (2017). Resistencia a la compresión de un concreto compactado con rodillo en diferentes tiempos de vibrado [Tesis de licenciatura, Universidad Privada del Norte]. Repositorio de la Universidad Privada del Norte. https://hdl.handle.net/11537/12739 (es_PE)
624.1834 SALD/R 2017 (es_PE)
https://hdl.handle.net/11537/12739
La presente tesis tiene; como objetivo determinar la resistencia a compresión de un concreto
compactado con rodillo en diferentes tiempos de vibrado. Para este estudio se utilizó agregados de
la cantera Roca Fuerte, ubicada en Baños del Inca y cemento Portland tipo I; se inició evaluando las
propiedades físicas y mecánicas de los agregados, de la cual se han analizado sus propiedades
físicas determinándose que su granulometría está dentro de los límites de acuerdo a la norma ASTM
C-33, su módulo de finura es 2.97, gravedad específica 2.82 gr/cm
, absorción 3.68%, peso unitario
suelto 1636.31 Kg/m
3
, peso unitario compactado 1753.49 Kg/m
3
3
y el contenido de humedad 8.84%
para agregado fino, de la misma manera para agregado grueso su módulo de finura es 7.88,
gravedad específica 2.66 gr/cm
3
, absorción 1.29%, peso unitario suelto 1443.78 Kg/m
, peso unitario
compactado 1512.99 Kg/m
y contenido de humedad 0.44%. Se realizó el diseño de concreto
mediante la metodología combinación de agregados para un f’c=280 kg/cm
3
una muestra patrón y
3 muestras adicionales a tres tiempos diferentes de vibrado 5 seg., 10seg. y 15 seg. evaluados en
3 periodos de curado 7, 14 y 28 días; determinándose que a 7 días de curado la resistencia
alcanzada fue de 244.45 kg/cm² con un tiempo de vibrado de 0 seg.; 281.03 kg/cm², al utilizar la
vibrocompactación en un tiempo de 5 seg., 292.52 kg/cm² al utilizar la vibrocompactación en un
tiempo de 10 seg. y por último 299.65 kg/cm² con un vibrocompactado de 15 seg.; para en un tiempo
de curado de 14 días la resistencia alcanzada fue de 287.00 kg/cm² con un tiempo de vibrado de 0
seg.; 298.40 kg/cm² al utilizar la vibrocompactación en un tiempo de 5 seg., 303.84 kg/cm² al utilizar
la vibrocompactación en un tiempo de 10 seg. y por último 327.15 kg/cm² con un vibrocompactado
de 15 seg. y para en un tiempo de curado de 28 días la resistencia alcanzada fue de 320.84 kg/cm²
con un tiempo de vibrado de 0 seg.; 337.15 kg/cm² al utilizar la vibrocompactación en un tiempo de
5 seg., 343.94 kg/cm² al utilizar la vibrocompactación en un tiempo de 10 seg. y por último 357.25
kg/cm² con un vibrocompactado de 15 seg. Concluyendo que a mayor tiempo de vibrado aumenta
la resistencia a compresión axial, la cual para una edad de 28 días de curado se incrementa 11.35%
su resistencia logrando incluso superar la resistencia a compresión axial de la probeta patrón. (es_PE)
The present thesis has; as an objective to determine the compressive strength of a concrete
compacted with a roller at different vibration times. For this study, aggregates from the Roca Fuerte
quarry, located in Baños del Inca and Portland cement type I, were used; was started by evaluating
the physical and mechanical properties of the aggregates, from which their physical properties have
been analyzed, determining that their granulometry is within the limits according to the ASTM C-33
standard, its fineness modulus is 2.97, specific gravity 2.82 gr / cm3, absorption 3.68%, loose unit
weight 1636.31 Kg / m3, compacted unit weight 1753.49 Kg / m3 and moisture content 8.84% for
fine aggregate, in the same way for coarse aggregate its fineness modulus is 7.88, specific gravity
2.66 gr / cm3, absorption 1.29%, loose unit weight 1443.78 Kg / m3, compacted unit weight 1512.99
Kg / m3 and moisture content 0.44%. The concrete design was carried out using the combination of
aggregates methodology for a f'c = 280 kg / cm2 a standard sample and 3 additional samples at
three different times of vibration 5 sec., 10sec. and 15 sec. evaluated in 3 healing periods 7, 14 and
28 days; determining that after 7 days of curing the resistance reached was 244.45 kg / cm² with a
vibration time of 0 sec .; 281.03 kg / cm², when using vibrocompaction in a time of 5 sec., 292.52 kg
/ cm² when using vibrocompaction in a time of 10 sec. and finally 299.65 kg / cm² with a
vibrocompacted 15 sec .; for a curing time of 14 days the resistance reached was 287.00 kg / cm²
with a vibration time of 0 sec .; 298.40 kg / cm² when using vibrocompaction in a time of 5 sec.,
303.84 kg / cm² when using vibrocompaction in a time of 10 sec. and finally 327.15 kg / cm² with a
vibrocompacted 15 sec. and for a curing time of 28 days the resistance reached was 320.84 kg / cm²
with a vibration time of 0 sec .; 337.15 kg / cm² when using vibrocompaction in a time of 5 sec.,
343.94 kg / cm² when using vibrocompaction in a time of 10 sec. and finally 357.25 kg / cm² with a
vibrocompacted 15 sec. Concluding that the greater the time of vibration the resistance to axial
compression increases, which for an age of 28 days of curing increases its resistance by 11.35%,
even exceeding the resistance to axial compression of the standard specimen. (es_PE)
Tesis (es_PE)
application/pdf (es_PE)
application/msword (es_PE)
spa (es_PE)
Universidad Privada del Norte (es_PE)
info:eu-repo/semantics/openAccess (es_PE)
https://creativecommons.org/licenses/by-nc-sa/3.0/us/ (*)
Universidad Privada del Norte (es_PE)
Repositorio Institucional - UPN (es_PE)
Resistencia a la compresión (es_PE)
Concreto (es_PE)
Materiales de construcción (es_PE)
Resistencia a la compresión de un concreto compactado con rodillo en diferentes tiempos de vibrado (es_PE)
info:eu-repo/semantics/bachelorThesis (es_PE)
Universidad Privada del Norte. Facultad de Ingeniería (es_PE)
Ingeniería Civil (es_PE)
Título Profesional (es_PE)
Ingeniero Civil (es_PE)
PE (es_PE)
https://purl.org/pe-repo/ocde/ford#2.01.01 (es_PE)
Pregrado (es_PE)
https://purl.org/pe-repo/renati/level#tituloProfesional (es_PE)
40208212
https://orcid.org/0000-0003-4203-7795 (es_PE)
46707832
732016 (es_PE)
Aguilar Aliaga, Orlando
Quispe Rodríguez, Gerson Neri
Alva Sarmiento, Anita Elizabet
https://purl.org/pe-repo/renati/type#tesis (es_PE)
Privada societaria
This item is licensed under a Creative Commons License